MKP 300V 10µF RM37,5 X2

pitch: 15...37.5mm

* dielectric polypropylene film. Aluminium layer plates deposited by evaporation under vacuum
* box material is solvent resistant and flame retardant (UL94V-0), no impregnation
* low attenuation
* low dissipation factor (tan d)
* high pulse strength (du/dt)
* high insulation resistance

MKP 300V 10µF RM37,5 X2

28145 MKP 300V 10µF RM37,5 X2 R463W510000M1M R463W510000M1M pitch: 15...37.5mm. * dielectric polypropylene film. Aluminium layer plates deposited by evaporation under vacuum* box material is solvent resistant and flame retardant (UL94V-0), no impregnation* low attenuation* low dissipation factor (tan d)* high pulse strength (du/dt)* high insulation resistance

Specifications

manufacturer
Manufacturer's name R463W510000M1M
Nominal voltage [V] 300
Pitch [mm] 37,5
Tolerance [%] 20
Capacity [pF] 10000000
Data Sheet

Unit price

3,59 €